Mechanical Properties Metric English Comments
Tear Strength 17.9 kN/m
102 pli
ASTM D624 Die B
Freudenberg Simrit S60 Silicone Elastomer (VMQ)
General Purpose; AMS 3301; A-A-59588 (ZZ-R-765) Class 2A, 2B Grade 40; Good heat resistance. Poor resistance to abrasion, tear and cut growth; low tensile strength; inferior resistance to oil, gasol..
Tear Strength 17.9 kN/m
102 pli
Trouser; ASTM D470
Lubrizol ESTANE® 58370 Ether Based Thermoplastic Polyurethane
Features: Halogenated flame retardant compoundUses: Extrusion – Wire and cable and general application where flame retardant properties are neededAvailable in Americas, Europe, Middle East, Africa,..
Tear Strength 17.9 kN/m
102 pli
Die C; ASTM D624
Lubrizol ESTANE® 58810 Ether Based Thermoplastic Polyurethane
Features: High melt flow and improved temperature resistanceUses: Extrusion – Wire and cable, Hose and tubeAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by ..