Mechanical Properties Metric English Comments
Tear Strength >= 19.26 kN/m
>= 109.9 pli
ASTM D624
Multibase Multi-Flex® TPE A 6221 M BLK
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tear Strength >= 19.26 kN/m
>= 109.9 pli
ASTM D624
Multibase Multi-Flex® TPE A 6006 GREY
Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Tear Strength >= 19.26 kN/m
>= 109.9 pli
ASTM D624
Multibase Multi-Flex® TPE A 6221 BLK
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Tear Strength >= 19.26 kN/m
>= 109.9 pli
ASTM D624
Multibase Multi-Flex® TPE A 6221 C GREY
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Tear Strength >= 19.26 kN/m
>= 109.9 pli
ASTM D624
Multibase Multi-Flex® TPE A 6221 LA BLK
Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Tear Strength >= 19.26 kN/m
>= 109.9 pli
ASTM D624
Multibase Multi-Flex® TPE A 6006 BLK
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tear Strength >= 19.26 kN/m
>= 109.9 pli
ASTM D624
Multibase Multi-Flex® TPE A 6221 NAT
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tear Strength >= 19.26 kN/m
>= 109.9 pli
ASTM D624
Multibase Multi-Flex® TPE A 6421 BLK
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.