Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 112 kN/m | 639 pli | ASTM D624 |
Multibase Multi-Flex® TPE D 5302 NAT The moisture content is 0.912%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 112 kN/m | 640 pli | ASTM D624 |
Huntsman IROGRAN® A 85 D 4968 Polyester-Based TPU-Injection Extrusion Grade High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman |
|||
Tear Strength | 112 kN/m | 639 pli | ASTM D624 DIE C |
Lubrizol Advanced Materials Pearlthane® 12T92E Thermoplastic Polyurethane Elastomer PEARLTHANE® 12T92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and low temperature performance. This gra.. |
|||
Tear Strength | 112 kN/m | 640 pli | ASTM D624 |
Multibase Multi-Flex® D 5308 848 Black TPO Thermoplastic Polyolefin Elastomer Forms: PelletsInformation provided by Multibase |
|||
Tear Strength | 112 kN/m | 639 pli | without incision; ISO 34B |
Lubrizol ESTANE® GP85AB Ester Based Thermoplastic Polyurethane Type: Estane® GP 85AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsInformation provided by Lubrizol. |
|||
Tear Strength | 112 kN/m | 639 pli | parallel; ISO 34-1 |
DuPont Performance Polymers Hytrel® HTR8685 BK022A Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Hytrel HTR8685 BK022A is designed for blow molding or processing techniques requi.. |