Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | >= 20.0 kN/m | >= 114 pli | DIN 53507 |
Karina E CAK 65-48/1 Black PVC Compound Reclaimed PVC compound recommended for soles injectionInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 20.0 kN/m | 114 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ Electro 242-0 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ FSL 7586/40 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ FSL 7641 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2070 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2345/05 Electrically-Conductive Liquid Silicone Rubber This LSR elastomer is an electrically conductive, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2620 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 4630 FC Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Tear Strength | 20.0 kN/m | 114 pli | Die B |
Momentive Performance Materials HV 3/806 Heat Cured Rubber - High Temperature Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg B429 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg Neoprene® C627 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg R408 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg R480 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg S864 Silicone Rubber PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering... |
|||
Tear Strength | 20.0 kN/m | 114 pli | ASTM D624 |
ELASTO UK Mediprene™ 660420M TPE, Medical Applications, 42A Hardness All Mediprene™ compounds are designed and manufactured for use in medical and pharmaceutical applications. In both medical and food contact areas, high application demands are found, such as:Low e.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | ASTM D624 |
ELASTO UK Mediprene™ 660440M TPE, Medical Applications, 44A Hardness All Mediprene™ compounds are designed and manufactured for use in medical and pharmaceutical applications. In both medical and food contact areas, high application demands are found, such as:Low e.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | Parallel to flow; ISO 34-B |
AlphaGary Evoprene™ LF 6151 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | Die B |
Momentive Performance Materials HV 3/706 Heat Cured Rubber - High Temperature Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | Trouser Tear resistance MD; ISO 6383-1 |
EMS-Grivory Grivory® L 25 nat PA12 Product Description: Grilamid L 25 is a high viscosity polyamide 12. This product has the following features: Very tasteless High toughness, even at low temperatures Good resistance to weathering Go.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | ISO 34-B |
AlphaGary Evoprene™ GC 5688 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |