Polymer Property : Tear Strength = 115 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 115 kN/m
656 pli
ISO 34B
Huntsman AVALON® 90 AB Thermoplastic Polyurethane
Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce..
Tear Strength 115 kN/m
656 pli
ISO 34B
Huntsman AVALON® 90 ABR Thermoplastic Polyurethane
Introduction: AVALON 90 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 90 ABR is part of the AVALON Performance Range and offers a premium soling ..
Tear Strength 115 kN/m
656 pli
ASTM D1004
SK Chemicals SKYPEL G140D General Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Tear Strength 115 kN/m
656 pli
ASTM D624
Wanhua Chemical Wanthane® WHT-1190 Polyester Based TPU
Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd.
Tear Strength 115 kN/m
656 pli
ASTM D624
Wanhua Chemical Wanthane® WHT-8254 Polyether-Based TPU
Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Tear Strength 115 kN/m
656 pli
ISO 34
Chengdu Polyster H4543 Thermoplastic Polyether-ester Elastomer (TPEE)
Low modulus molding and injection grade. Contains improved color- stable antioxidants. Applications requiring high original color retention. Molded and injected products for consumer use, such as se..
Tear Strength 115 kN/m
656 pli
notched; ASTM D624 (C)
Arkema Group Pebax® 5533 Polyether Block Amide (PEBA)
Information provided by Arkema Group
Tear Strength >= 115 kN/m
>= 656 pli
ISO 34
Austin Novel Materials Texalan® 295A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Tear Strength 115 kN/m
654 pli
Die C
ACC SMP™ EP 82 EPI Engineered Polymers Silicone Modified Polyurea
EP 82, “Powered by Reactamine® Technology”, is a new hydrophobic silicone polyurea. The product is characterized by its low viscosity and ability to readily blend with polyisocyanates. It may be ..
Tear Strength 115 kN/m
656 pli
ASTM D624
BASF Elastollan® 690A15N Polyester Type Polyurethane Elastomer
This grade is FDA compliant, section 177.2600 and 177.1680, for both wet and dry contact with food. The Elastollan 600 Series of products listed are products that are part of a new series of polyes..