Polymer Property : Tear Strength = 12.8 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 12.8 kN/m
73.0 pli
ASTM D624
Multibase Multi-Flex® A 0840 Black TPE Thermoplastic Elastomer
Forms:PelletsProcessing Method:Injection Molding Information provided by Multibase
Tear Strength 12.8 kN/m
73.0 pli
Dow Corning SILASTIC® 591 LSR PART A&B
50 Durometer, 2-part, 1 to 1 mix, off-white, Liquid Silicone Rubber, for insulating sleeve and printing roller appliacations.Information provided by Dow Corning
Tear Strength 12.8 kN/m
73.0 pli
Die C; ASTM D 624
CPT C-Flex® R70-214 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Tear Strength 12.8 kN/m
73.0 pli
Die B, Silicone Property; ASTM D624
Arlon R38026B017 0.017" (0.432 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1165 FiberglassSide 2: Uncured Silicone Rubber Interleave: LDPEThis data represents typical values for the production material. The..
Tear Strength 12.8 kN/m
73.0 pli
Die B, Silicone Property; ASTM D624
Arlon R38020B020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: LDPESide 1: Uncured Silicone RubberSubstrate: Style 1165 FiberglassThis data represents typical values for the production material. The data should not be used to wr..