Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 23.0 kN/m | 131 pli | D624 |
Polykemi AB POLYelast TPE Z600 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Tear Strength | 23.0 - 26.0 kN/m | 131 - 148 pli | NF EN ISO 1421 |
Isoflon Tisoflon® 5G Polytetrafluoroethylene & Graphite Coated Glass Fabric PTFE + Graphite coated glass fabric TISOFLON® - Black anti-staticInformation provided by Isoflon. |
|||
Tear Strength | 23.0 kN/m | 131 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ FFSL 7051 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Tear Strength | 23.0 - 24.0 kN/m | 131 - 137 pli | NF EN ISO 1421 |
Isoflon Tisoflon® 10S Silicone Coated Glass Fabric Silicone coated Glass fabric TISOFLON®Information provided by Isoflon. |
|||
Tear Strength | 23.0 - 26.0 kN/m | 131 - 148 pli | NF EN ISO 1421 |
Isoflon Tisoflon® 5 AD Polytetrafluoroethylene Coated Glass Fabric PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon. |
|||
Tear Strength | 23.0 kN/m | 131 pli | Die B |
Momentive Performance Materials TSE 221-5U Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 23.0 kN/m | 131 pli | Press-cured 5 minutes at 190°C; ISO 34 |
DuPont Vamac® DP HVA-2 Coagent Test Compound Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper.. |
|||
Tear Strength | 23.0 kN/m | 131 pli | |
Trelleborg E550 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Tear Strength | 23.0 kN/m | 131 pli | |
Trelleborg E669 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Tear Strength | 23.0 kN/m | 131 pli | GB/T 529 |
Chengdu Polyster FR2075 Flame Retardant Grade TPV Good heat stability and light stability. Meets the requirements of European Dioxine Principle and the environmental protection criteria. Can be used for wires, cables, buncles, carcass of train.Inf.. |
|||
Tear Strength | 23.0 kN/m | 131 pli | Method C; ISO 34 |
ELASTO UK Dryflex® 8006-101 Flame Retardant TPE for Extrusion, Black, Halogen Free Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and.. |
|||
Tear Strength | 23.0 kN/m | 131 pli | Method C; ISO 34 |
ELASTO UK Dryflex® 8006-101 Flame Retardant TPE for Extrusion, Natural, Halogen Free Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and.. |
|||
Tear Strength | 23.0 kN/m | 131 pli | Method C; ISO 34 |
ELASTO UK Dryflex® 8006-101 Flame Retardant TPE for Injection Molding, Black, Halogen Free Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu.. |
|||
Tear Strength | 23.0 kN/m | 131 pli | 73°F, Die C, Across Flow; ASTM D624 |
ExxonMobil Santoprene® 171-64 Thermoplastic Elastomer A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Tear Strength | 23.0 kN/m | 131 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 201-64 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Tear Strength | 23.0 kN/m | 131 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 271-64 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Tear Strength | 23.0 kN/m | 131 pli | Die B; Silicone Property; ASTM D624 |
Arlon T4020-R002 0.020" Cured, Fusible Silicone Rubber with Fiberglass Substrate 0.5 inch wide, 20 mil thick, red, rectangular cross-section, fusible silicone tape.Design/Construction:Side 1: Cured Fusible Silicone RubberSubstrate: 15% Sinusoidal FiberglassSide 2: Cured Fusibl.. |
|||
Tear Strength | 23.0 kN/m | 131 pli | |
ACC MM928 Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing.. |
|||
Tear Strength | 23.0 kN/m | 131 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Vyram™ 9201-55 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Tear Strength | 23.0 kN/m | 131 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 221-64W175 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed .. |