Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 27.8 kN/m | 159 pli | ISO 34 |
Multibase TPSiV® 4200-60A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
Tear Strength | 27.9 kN/m | 159 pli | Die C, Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4520 General Purpose Compound FormulationNordel® IP 4520 |
|||
Tear Strength | 27.8 kN/m | 159 pli | Die C, Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4640 Molded Golf Grips FormulationNordel® IP 4640 |