Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 30.1 kN/m | 172 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Elastamax™ HTE 3060 Polyvinyl Chloride + NBR (PVC+NBR) Elastamax™ HTE Series thermoplastic elastomers (TPEs) are based upon compounded blends of PVC resins and nitrile rubber. These elastomeric materials provide outstanding resistance to hydrocarbons a.. |