Polymer Property : Tear Strength = 176 kN/m
Polymer Property :
Tear Strength =
176 kN/m
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tear Strength
176
kN/m
1000
pli
ASTM D624
Toyobo PELPRENE™ P150B-05 Polyester TPE, Non-smell, Non-deposit
Features: Polyester TPE, Non-smell, Non-depositInformation provided by Toyobo.