Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 33.1 kN/m | 189 pli | Die C |
NEU NeuSoft™ 455-50A Ester/ether TPU / SBC blend |
|||
Tear Strength | 33.1 kN/m | 189 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR MBTS MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 33.2 kN/m | 189 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.25 PHR Zinc Stearate MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 33.2 kN/m | 189 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.25 PHR Zinc Stearate MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 33.1 kN/m | 189 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR MBTS MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 33.1 kN/m | 189 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7380-9000 TPE Product Description: StarFlex P 7380-9000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelGood WeatherabilityFDA and medical grades availableProcessing Method.. |