Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 2.29 kN/m | 13.1 pli | JIS K6301-B |
Stellarchem GP-975B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |