Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 25.7 kN/m | 147 pli | ASTM D624 |
PolyOne Versaflex™ HC 2110-57B Thermoplastic Elastomer (TPE) Versaflex™ HC 2110-57B is a TPE designed for use in the healthcare industry offering low stiction and good compression set. New Product. Commercial specifications have not been established. - Bonds.. |
|||
Tear Strength | 25.7 kN/m | 147 pli | Die C |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 15.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Tear Strength | 25.7 kN/m | 147 pli | Die C |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 15.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |