Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 26.2 kN/m | 149 pli | ISO 34 |
Multibase TPSiV® 4200-50A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
Tear Strength | 26.2 kN/m | 149 pli | Die C, 2 in/min; ASTM D1004 |
PolyOne Geon™ Vinyl Flexible 86143 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Tear Strength | 26.2 kN/m | 149 pli | Die C; ASTM D624 |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Friction Compound MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 26.2 kN/m | 149 pli | Die C; ASTM D624 |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Friction Compound MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |