Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 46.5 kN/m | 265 pli | post cured- 2 hours at 177°C; Die B |
Multibase SILASTIC® Q7-4750 Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 46.4 kN/m | 265 pli | ASTM D624 |
PolyOne Dynaflex™ G7690-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7690-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Tear Strength | 46.4 kN/m | 265 pli | ASTM D624 |
PolyOne Dynalloy™ 8900-80 Thermoplastic Elastomer (TPE) Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen.. |
|||
Tear Strength | 46.4 kN/m | 265 pli | ASTM D624 |
PolyOne Dynaflex™ G7690-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7690-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Tear Strength | 46.4 kN/m | 265 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 46.4 kN/m | 265 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 46.4 kN/m | 265 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 46.4 kN/m | 265 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 80 PHR Dixie Clay Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 46.5 kN/m | 265 pli | Die C; ASTM D624 |
Teknor Apex Flexalloy® 3500-75NT Polyvinyl Chloride Elastomer Features: Good Thermal Stability; Recyclable Material; Good Weather Resistance; Ultra High Molecular Weight Uses: Medical/Healthcare Applications; Pump Parts; Tubing Agency Ratings: FDA Unspecified .. |
|||
Tear Strength | 46.5 kN/m | 265 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 10 Basic PTFE-Coated Glass Description: Chemfab® Basic Series products are low resin-content, non-porous, PTFE-coated fiberglass fabrics. Applications are spray shields, separator sheets, release sheets and protective barr.. |
|||
Tear Strength | 46.5 kN/m | 265 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 10 Industrial PTFE-Coated Glass Description: Chemfab® Industrial Series products are multi-purpose, non-porous, medium-resin content, PTFE-coated fiberglass fabrics. Applications include release sheets, packaging, composites, g.. |
|||
Tear Strength | 46.4 kN/m | 265 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 80 PHR Dixie Clay Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 46.4 kN/m | 265 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 46.5 kN/m | 265 pli | |
Dow Corning SILASTIC® LS 5-2060 FLUOROSILICONE RUBBER 60 Durometer, off-white, molding grade fluorosilicone base.Information provided by Dow Corning |
|||
Tear Strength | 46.4 kN/m | 265 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 46.4 kN/m | 265 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |