Mechanical Properties Metric English Comments
Tear Strength 46.8 kN/m
267 pli
ASTM D624
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7190-1000 TPE
Product Description: StarFlex P 7190-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai..