Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 47.0 kN/m | 268 pli | Die B,post cured- 2 hours at 200°C; ASTM D624 |
Multibase SILASTIC® 7-6840 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tear Strength | 47.0 kN/m | 268 pli | as molded; Die B |
Multibase SILASTIC® C7-4565 CADOX TS-50S Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 47.0 kN/m | 268 pli | Die B |
Momentive Performance Materials TUFELâ„¢ II 94505 Low Volatile Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 47.0 kN/m | 268 pli | Die B |
Momentive Performance Materials TUFELâ„¢ II 94506 Low Volatile Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 47.0 kN/m | 268 pli | ASTM D624 |
UBE UBEPOL BR100 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
Tear Strength | 47.0 kN/m | 268 pli | ASTM D624 |
UBE UBEPOL BR150 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
Tear Strength | 47.0 kN/m | 268 pli | ASTM D2240 |
UBE UBEPOL BR153A Oil-Extended BR Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
Tear Strength | 47.0 kN/m | 268 pli | ASTM D624 |
UBE UBEPOL VCR150 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
Tear Strength | 47.0 kN/m | 268 pli | GB/T 529 |
Chengdu Polyster 7500 General Grade TPV Information provided by Chengdu Polyster Co., Ltd. |
|||
Tear Strength | 47.0 kN/m | 268 pli | Die C; ASTM D 624 |
CPT C-Flex® R70-089 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Tear Strength | 47.0 kN/m | 268 pli | 73°C, Die C; ASTM D624 |
ExxonMobil Santoprene® 8281-90MED Thermoplastic Elastomer A hard, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Tear Strength | 47.0 kN/m | 268 pli | ISO 34-B |
AlphaGary Evoprene™ 032 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Tear Strength | 47.0 kN/m | 268 pli | ASTM D1004 |
Bayshore Vinyl Compounds BVC 1100-65 Clear PVC Compound BVC 1100-65 is a clear flexible PVC compound produced with FDA sanctioned ingredients. It is recommended for use in applications for the medical, food and beverage industries. This material offers.. |
|||
Tear Strength | 47.0 kN/m | 268 pli | Parallel to flow; ISO 34-B |
AlphaGary Evoprene™ LF 6156 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |