Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 48.4 kN/m | 276 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarXTRUDE XTR-85-1000 TPE Product Description: StarXTRUDE XTR-85-1000 is an easy processing TPE designed for extrusion. Features:Soft TouchRubbery FeelMatte finishExcellent chemical and oil resistanceAdherence to PC, ABS & P.. |