Mechanical Properties Metric English Comments
Tear Strength 3.16 kN/m
18.0 pli
Die C; ASTM D624
Northstar Polymers MPP-V37A Polyurethane Gel Elastomer
This two-component polyurethane casting system makes type of soft elastomer material known as “gel”. Applications for this material include filling component for computer keyboard/mouse-pad wrist..
Tear Strength 3.16 kN/m
18.0 pli
Die C; ASTM D624
Monmouth Rubber & Plastics Durafoamâ„¢ C41 Closed Cell Epichlorohydrin
Information provided by Monmouth Rubber & Plastics Corp.