Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 0.596 kN/m | 3.40 pli | Split Tear Resistance |
Northstar Polymers MPS-F08A Hand-Mixable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or machine casting by the meter dispensing equipment. The components are stable and liquid at .. |