Tear Strength 55.3 kN/m
316 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.5 PHR Sulfur
Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man..
Tear Strength 55.3 kN/m
316 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.5 PHR Sulfur
Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man..