Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 61.0 kN/m | 348 pli | ASTM D624-95 |
Multibase Multi-Flex® TPO D-6208 Data provided by Multibase. |
|||
Tear Strength | 61.0 kN/m | 348 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR MBTS MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 61.0 kN/m | 348 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR MBTS MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 61.0 kN/m | 348 pli | without incision; ISO 34B |
Lubrizol ESTANE® GP70AE Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 61.0 kN/m | 348 pli | M.D., Split Tear @ 254 mm/min; ASTM D1938 |
Eastman Eastman Embrace Copolyester for Extrusion/Cast Film Applications:Flexible packagingIV containersLabels to fit high contour containersShrink packagingWrap around designKey Attributes:Excellent clarityExcellent printabilityGood chemical resistanceGood .. |
|||
Tear Strength | 61.0 kN/m | 348 pli | T.D., Split Tear @ 254 mm/min; ASTM D1938 |
Eastman Eastman Embrace Copolyester for Extrusion/Cast Film Applications:Flexible packagingIV containersLabels to fit high contour containersShrink packagingWrap around designKey Attributes:Excellent clarityExcellent printabilityGood chemical resistanceGood .. |
|||
Tear Strength | 61.0 kN/m | 348 pli | ISO 34-B |
AlphaGary Evoprene™ 029 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Tear Strength | 61.0 kN/m | 348 pli | ISO 34-B |
AlphaGary Evoprene™ HP 3730 High Performance Thermoplastic Elastomer Evoprene™ HP is a hydrogenated styrene block copolymer based thermoplastic elastomer. Specially formulated for applications requiring high strength and excellent abrasion resistance, Evoprene™ HP.. |