Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 64.6 kN/m | 369 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 9007 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 64.7 kN/m | 369 pli | Die C; ASTM D624 |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 0.0 PHR Caytur 4 MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 64.7 kN/m | 369 pli | Die C; ASTM D624 |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 0.0 PHR Caytur 4 MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 64.7 kN/m | 369 pli | Die C; ASTM D624 |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, No Milling Time MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 64.7 kN/m | 369 pli | Die C; ASTM D624 |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, No Milling Time MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |