Mechanical Properties Metric English Comments
Tear Strength 38.7 kN/m
221 pli
as molded; Die B
Multibase SILASTIC® C7-4565 TBPB Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tear Strength 38.7 kN/m
221 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N339 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 38.7 kN/m
221 pli
Die C
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Fumed Silica - Wacker HK N20
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tear Strength 38.7 kN/m
221 pli
Die C
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Fumed Silica - Wacker HK N20
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tear Strength 38.7 kN/m
221 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N330 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 38.7 kN/m
221 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N339 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 38.7 kN/m
221 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N330 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..