Polymer Property : Tear Strength = 38.8 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 6.80 kN/m
38.8 pli
Die B
Momentive Performance Materials RTV577 White Extreme Low Temperature Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..