Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 39.1 kN/m | 223 pli | Die C |
NEU NeuSoft™ 596-50A Medical Ether TPU / SBC blend |
|||
Tear Strength | 39.1 kN/m | 223 pli | Die B |
Shin-Etsu Silicones KEG-2001-70A/B Fast Curing LIMS Silicone Rubber ShinEtsu KEG200170 is a very fast cure liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. The viscosity of KEG20.. |
|||
Tear Strength | 39.1 kN/m | 223 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 75-LR-9 TPE Product Description: StarTUFF TF 75-LR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
Tear Strength | 39.1 kN/m | 223 pli | Die B, no post cure; ASTM D624 |
Multibase C6-180 Dow-Corning Class VI Elastomer Information provided by Multibase |