Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 6.96 kN/m | 39.8 pli | |
Momentive Performance Materials RTV5812 One-Component, Modified Alkoxy Adhesive Sealant, White RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Tear Strength | 6.96 kN/m | 39.8 pli | |
Momentive Performance Materials RTV5813 One-Component, Modified Alkoxy Adhesive Sealant, Black RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Tear Strength | 6.96 kN/m | 39.8 pli | |
Momentive Performance Materials RTV5818 One-Component, Modified Alkoxy Adhesive Sealant, Translucent RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |