Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 390 kN/m
2230 pli
ASTM D624
GRECO ISOTHANE 3075A Polyether TPU Resin
ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod..
Tear Strength 390 kN/m
2230 pli
machine direction; ASTM D1922A
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin
DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl..
Tear Strength 390 kN/m
2230 pli
machine direction; ASTM D1922A
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin
DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl..
Tear Strength 390 kN/m
2230 pli
machine direction; ASTM D1922A
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin
DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl..
Tear Strength 390 kN/m
2230 pli
machine direction; ASTM D1922A
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin
DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl..
Tear Strength 390 kN/m
2230 pli
machine direction; ASTM D1922A
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin
DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl..
Tear Strength 390 kN/m
2230 pli
machine direction; ASTM D1922A
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin
DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl..