Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 69.6 kN/m | 397 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 69.6 kN/m | 397 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 69.6 kN/m | 397 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 69.6 kN/m | 397 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |