Tear Strength 4.10 kN/m
23.4 pli
ISO 34-C
Premix Thermoplastics PRESEAL® TPE 5010
PRESEAL TPE 5010 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It may also find interesting uses as conductors or in grounding applica..
Tear Strength 4.10 kN/m
23.4 pli
ISO 34-C
Premix Thermoplastics PRESEAL® TPE 5020
General Description:PRESEAL® TPE 5020 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It may also find interesting uses as conductors o..
Tear Strength 4.10 kN/m
23.4 pli
ISO 34-C
Premix Thermoplastics PRESEAL® TPE 6080
General Description:PRESEAL® TPE 6080 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It can also be used as conductors or in grounding..