Polymer Property : Tear Strength = 4.40 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 4.40 kN/m
25.1 pli
Typical; ASTM D264-91 Die C
Rogers Corporation Poron® 4701-50 Thin as Cast Urethane Foam, Firm, Thin as Cast
Firm material used for managing high energy impact with gasketing needs.  Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce..