Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 7.27 kN/m | 41.5 pli | propogation; ASTM D1922 |
SABIC Innovative Plastics Lexan® FR700 Polycarbonate Film, Flame Retardant Lexan FR700 is a black, one side fine matt, one side velvet flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good d.. |
|||
Tear Strength | 7.27 kN/m | 41.5 pli | propogation; ASTM D1922 |
SABIC Innovative Plastics Lexan® FR735A Polycarbonate Film, Flame Retardant Lexan FR735A is a black, one side velvet, one polish flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good dimensio.. |
|||
Tear Strength | 7.27 - 316 kN/m | 41.5 - 1800 pli | Average value: 143 kN/m Grade Count:7 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |