Polymer Property : Tear Strength = 468 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 82.0 kN/m
468 pli
ISO 34-1B
Lubrizol Advanced Materials Pearlthane® D91T80 Thermoplastic Polyurethane
Type : Pearlthane® D91T80 is a aliphatic-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Low density, fast processing and excellent elasticity properties...
Tear Strength 82.0 kN/m
468 pli
without incision; ISO 34B
Lubrizol ESTANE® GP80AE Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tear Strength 82.0 kN/m
468 pli
Die C; ASTM D624
Covestro Bayflex® 110-80 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o..