Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 83.4 - 123 kN/m | 476 - 700 pli | |
Taiwan PU Corporation PPG CPU-1090C Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |
|||
Tear Strength | 83.4 kN/m | 476 pli | ASTM D624 |
SK Chemicals SKYTHANE® 310 Hotmelt Grade UB Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tear Strength | 83.4 kN/m | 476 pli | ASTM D624 |
SK Chemicals SKYTHANE® UB310 Co-Extruding Adhesive Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta.. |
|||
Tear Strength | 83.4 kN/m | 476 pli | Die C; ASTM D624 |
Teknor Apex Telcar® TL-1182A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tear Strength | 83.4 kN/m | 476 pli | ASTM D624 |
SK Chemicals SKYTHANE® 370A T series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |