Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 83.6 kN/m | 477 pli | Die C |
ACC SMP™ EP 82 EPI Engineered Polymers Silicone Modified Polyurea EP 82, “Powered by Reactamine® Technology”, is a new hydrophobic silicone polyurea. The product is characterized by its low viscosity and ability to readily blend with polyisocyanates. It may be .. |