Mechanical Properties Metric English Comments
Tear Strength 84.1 kN/m
480 pli
Die C, 510 mm/min; ASTM D624
PolyOne Geon™ Vinyl Flexible B5DU0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tear Strength 84.1 kN/m
480 pli
ASTM Die C
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 25 PHR Tricresyl Phosphate
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
Tear Strength 84.1 kN/m
480 pli
Die C, 510 mm/min; ASTM D624
PolyOne Geon™ Vinyl Flexible B5D00 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tear Strength 84.1 kN/m
480 pli
Die C, 510 mm/min; ASTM D624
PolyOne Geon™ Vinyl Flexible B5D02 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tear Strength 84.1 kN/m
480 pli
Die C, 510 mm/min; ASTM D624
PolyOne Geon™ Vinyl Flexible B5DG1 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tear Strength 84.1 kN/m
480 pli
ASTM D624
Huntsman IROGRAN® A 80 P 5039 TPU-Polyether
Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman
Tear Strength 84.1 kN/m
480 pli
ASTM D790
LG Chemical KEYFLEX TO-1045D Thermoplastic Olefin for Injection Molding, 45D Hardness
KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber ..
Tear Strength 84.1 kN/m
480 pli
ASTM D624
Multibase Multi-Flex® G 7940 TPE Styrene Ethylene Butylene Styrene Block Copolymer
Features: Chemical Resistance, Good General PurposeOzone Resistant Thermal Stability, Good Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInfor..
Tear Strength 84.1 kN/m
480 pli
ASTM D624
Multibase Multi-Flex® D 3104 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsI..
Tear Strength 84.1 kN/m
480 pli
ASTM Die C
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 25 PHR Tricresyl Phosphate
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
Tear Strength 84.1 kN/m
480 pli
ASTM D412
ACC EP RAP 45 EPI Engineered Polymers Aliphatic Polyurea
EP RAP 45 Aliphatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC is, aliphatic polyurea (silicone optional) coating, that was developed for UV stable (col..
Tear Strength 84.1 kN/m
480 pli
ASTM D412
ACC EP RAP 45 14 EPI Engineered Polymers Aliphatic Polyurea
EP RAP 45 14 Aliphatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC’s, aliphatic polyurea coating that was developed for UV stable (colorfast) polyurea f..