Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 49.3 kN/m | 281 pli | Notched, Die B; ASTM D 624 |
CPT C-Flex® R70-089 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |