Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 5.00 kN/m | 28.5 pli | Support Sponge |
Fujipoly Industries Zebra® 1002 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tear Strength | 5.00 kN/m | 28.5 pli | Support Sponge |
Fujipoly Industries Zebra® 1002 Carbon Sponge Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tear Strength | 5.00 kN/m | 28.5 pli | Support Sponge |
Fujipoly Industries Zebra® 2004 Carbon Sponge Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tear Strength | 5.00 kN/m | 28.5 pli | Support Sponge |
Fujipoly Industries Zebra® 2005 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tear Strength | 5.00 kN/m | 28.5 pli | Support Sponge |
Fujipoly Industries Zebra® 2005 Carbon Sponge Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tear Strength | 5.00 kN/m | 28.5 pli | Support Sponge |
Fujipoly Industries Zebra® LT 200 Low Temperature Carbon Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tear Strength | 5.00 kN/m | 28.5 pli | Die B |
Momentive Performance Materials RTV31 Red Extreme High Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Tear Strength | 5.00 kN/m | 28.5 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2080 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 5.00 kN/m | 28.5 pli | Support Sponge |
Fujipoly Industries Zebra® 2004 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tear Strength | 5.00 kN/m | 28.5 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 4080 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Tear Strength | 5.00 kN/m | 28.5 pli | Trouser Tear resistance MD; ISO 6383-1 |
EMS-Grivory Grivory® G 25 PA6I/6T Product description: Grivory G 25 is a very high viscous amorphous copolyamide. It is suitable for injection stretch blow molding, injection blow molding, extrusion blow molding, the manufacture of .. |
|||
Tear Strength | 5.00 kN/m | 28.5 pli | Trouser Tear resistance TD; ISO 6383-1 |
EMS-Grivory Grivory® G 25 PA6I/6T Product description: Grivory G 25 is a very high viscous amorphous copolyamide. It is suitable for injection stretch blow molding, injection blow molding, extrusion blow molding, the manufacture of .. |
|||
Tear Strength | 5.00 kN/m | 28.5 pli | Trouser Tear resistance MD; ISO 6383-1 |
EMS-Grivory Grivory® G 21 PA6I/6T Product description: Grivory G 21 natural 6506 is a high viscosity, partially aromatic, amorphous copolyamide with processing aid. Improved gas and aroma barrier at elevated relative humidityExcelle.. |
|||
Tear Strength | 5.00 kN/m | 28.5 pli | Trouser Tear resistance TD; ISO 6383-1 |
EMS-Grivory Grivory® G 21 PA6I/6T Product description: Grivory G 21 natural 6506 is a high viscosity, partially aromatic, amorphous copolyamide with processing aid. Improved gas and aroma barrier at elevated relative humidityExcelle.. |
|||
Tear Strength | 5.00 kN/m | 28.5 pli | Trouser Tear resistance MD; ISO 6383-1 |
EMS-Grivory Grivory® G 16 PA6I/6T Product description: Grivory G 16 is a low viscosity amorphous copolyamide. It is suitable for injection - stretch blow molding, injection blow molding, extrusion blow molding, the manufacture of co.. |
|||
Tear Strength | 5.00 kN/m | 28.5 pli | Trouser Tear resistance TD; ISO 6383-1 |
EMS-Grivory Grivory® G 16 PA6I/6T Product description: Grivory G 16 is a low viscosity amorphous copolyamide. It is suitable for injection - stretch blow molding, injection blow molding, extrusion blow molding, the manufacture of co.. |