Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 99.8 kN/m | 569 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 99.8 kN/m | 569 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |