Tear Strength 5.20 - 10.4 kN/m

@Temperature 150 - 150 °C
29.7 - 59.3 pli

@Temperature 302 - 302 °F
Average value: 8.16 kN/m Grade Count:5
Overview of materials for Thermoset Fluoroelastomer
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr..