Mechanical Properties Metric English Comments
Tear Strength 6.20 kN/m
35.4 pli
ASTM D470
DuPont Elvax® 40L-03 High Temperature Ignition Cable Jacket Formulation  (discontinued **)
Elvax® 40L-03 high temperature ignition cable jacket.Information provided by DuPont.
Tear Strength 6.20 kN/m
35.4 pli
ASTM D470
DuPont Elvax® 40L-08 High Temperature Ignition Cable Jacket Formulation  (discontinued **)
Elvax® 40L-08 high temperature ignition cable jacket.Information provided by DuPont.