Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 61.2 kN/m | 349 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 60A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 61.2 kN/m | 349 pli | ASTM Die C |