Polymer Property : Tear Strength = 62.1 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 62.1 kN/m
354 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, Hardness 93A
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 62.1 kN/m
354 pli
0.025" extruded film; ASTM D624
Huntsman IROGRAN® PS442-202 TPU-Polyester
Introduction: IROGRAN PS440-202 is a high performance polyester based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN PS440-202 is part of the HUNTSMAN ..
Tear Strength 62.1 kN/m
354 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, Hardness 93A
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..