Tear Strength 66.0 kN/m
377 pli
with incision; ISO 34B
Lubrizol ESTANE® GP80AB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 80AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Tear Strength 66.0 kN/m
377 pli
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Carbon Black, N-550 (FEF)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 66.0 kN/m

@Thickness 0.760 mm
377 pli

@Thickness 0.0299 in
Split tear strength; extruded sheet; ASTM D1938
BASF Elastollan® 1185A10W Wire & Cable Grade Polyurethane Elastomer
As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.
Tear Strength 66.0 kN/m

@Thickness 0.760 mm
377 pli

@Thickness 0.0299 in
Split tear strength; extruded sheet; ASTM D-1938
BASF Elastollan® 1185A10X Wire & Cable Grade Polyurethane Elastomer
Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.
Tear Strength 66.0 kN/m
377 pli
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Carbon Black, N-550 (FEF)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 66.0 kN/m

@Thickness 0.760 mm
377 pli

@Thickness 0.0299 in
Split tear strength; extruded sheet; ASTM D-1938
BASF Elastollan® 1185A10U Wire & Cable Grade Polyurethane Elastomer
As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.
Tear Strength 66.0 kN/m

@Thickness 0.760 mm
377 pli

@Thickness 0.0299 in
Split tear strength; extruded sheet; ASTM D-1938
BASF Elastollan® 1185A10V Wire & Cable Grade Polyurethane Elastomer
Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.
Tear Strength 66.0 kN/m

@Thickness 0.760 mm
377 pli

@Thickness 0.0299 in
Split tear strength; extruded sheet; ASTM D1938
BASF Elastollan® 1185A10Y Wire & Cable Grade Polyurethane Elastomer
Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.