Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tear Strength = 67.4 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 67.4 kN/m
385 pli
Across Flow; ASTM D624
PolyOne Versalloy™ HC 9220-90 Thermoplastic Elastomer (TPE)
Versalloy™ HC 9220-90 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr..
Tear Strength 67.4 kN/m
385 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 50 PHR N220 (ISAF) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 67.4 kN/m
385 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 50 PHR N220 (ISAF) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Copyright © lookpolymers.com All Rights Reserved