Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 117 kN/m | 670 pli | ASTM D624 |
Multibase Multi-Flex® G 7890 TPE Styrene Ethylene Butylene Styrene Block Copolymer Features: Chemical Resistance, Good General PurposeOzone Resistant Thermal Stability, Good Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInfor.. |