Tear Strength 7.50 kN/m
42.8 pli
ISO 6383
SABIC Innovative Plastics NORYL WCA871 PPE-TPE (Asia Pacific)
Halogen-free flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as insulation and cable jacket. Flame retardant performance and mechanical properties capable..