Polymer Property : Tear Strength = 7.80 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 7.80 kN/m
44.5 pli
ASTM D624
GRECO ISOTHANE 1680AE Polyether TPU Resin
ISOTHANE 1600 series products are polyether based thermoplastic polyurethanes with good balanced qualities. They exhibit high moisture vapor transmission. The product can be e xtruded and blowed.Inf..