Polymer Property : Tear Strength = 713 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 125 kN/m
713 pli
Die B
Momentive Performance Materials FQE206U Heat Cured Fluorosilicone Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 125 kN/m
713 pli
without incision; ISO 34B
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tear Strength 125 kN/m
713 pli
DIN 53515
Lubrizol ESTANE® 5722 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tear Strength 125 kN/m
713 pli
with incision; ISO 34B
Lubrizol ESTANE® 58133 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tear Strength 125 kN/m
713 pli
DIN ISO 34-1/Bb
BASF Elastollan 1198 A TPUR
Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi..
Tear Strength 125 kN/m
713 pli
ASTM D624
BASF Elastollan® 1190A Polyether Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes...
Tear Strength 125 kN/m
713 pli
ASTM D624
BASF Elastollan® S90A Polyester Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fue..
Tear Strength 125 kN/m
713 pli
ASTM D624
Wanhua Chemical Wanthane® WHT-2195 Polycaprolactone Based TPU
Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.