Mechanical Properties Metric English Comments
Tear Strength 73.5 kN/m
420 pli
ASTM D624
Kolon ELLAS K-475A Ester Based Thermoplastic Polyurethane
ApplicationsExtrusionInjectionIndustry PartsParts for Automobile/Mobile phoneInformation provided by API-Kolon.
Tear Strength 73.5 - 113 kN/m
420 - 644 pli
Taiwan PU Corporation PPG CPU-2079 Polyurethane Casting Elastomer
A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu..
Tear Strength 73.5 - 113 kN/m
420 - 644 pli
Taiwan PU Corporation PTMG CPU-100L Polyurethane Casting Elastomer
A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu..
Tear Strength 73.5 kN/m
420 pli
ASTM D624
SK Chemicals SKYTHANE® 465A T series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tear Strength 73.5 kN/m
420 pli
Die C; ASTM D624
Lubrizol Estane® T470A Thermoplastic Polyurethane
Type: Estane® T470A is a Shore 77A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b..
Tear Strength 73.5 kN/m
420 pli
500 mm/min; ASTM D 624
Zylog Neoplast® 250 FT EB Thermoplastic Vulcanizate
Neoplast 250 FT EB is a hard, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro..
Tear Strength 73.5 kN/m
420 pli
ASTM D624
SK Chemicals SKYTHANE® 365A T series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..